N
|
Technical Parameters
|
Unit
|
|||||
1
|
Surface densoty (weight)
|
g/m2
|
475±5%
|
350±5%
|
300±5%
|
260±5%
|
210±5%
|
2
|
Thickness
|
mm
|
0.55±5%
|
0.35±5%
|
0.30±5%
|
0.29±5%
|
0.26±5%
|
3
|
Width
|
mm
|
2000±1%
|
1200±1%
|
1200±1%
|
1200±1%
|
1200
|
4
|
Kind of interweaving
|
L
|
L
|
L
|
L
|
L
|
|
5
|
Density (warp)
|
yarn/cm
|
4.5
|
7
|
4.4
|
7
|
5
|
(weft)
|
yarn/cm
|
3.5
|
6
|
7.0
|
7.5
|
6
|
|
6
|
Warp tex (warp)
|
tex
|
600X1
|
70X4
|
140X2
|
125X2 Twisted
|
125X2 Twisted
|
Weft tex (weft)
|
tex
|
600X1
|
70X4
|
140X2
|
125 Roving
|
125X1 Roving
|
|
7
|
Tensile strenght (warp)
|
N/50mm
|
4600±5%
|
3800±5%
|
470±5%
|
2360±5%
|
1670±5%
|
(weft)
|
N/50mm
|
4100±5%
|
3000±5%
|
170±5%
|
950±5%
|
825±5%
|
|
8
|
temperature range of exploitation
|
°C
|
(-267) ... (+850)
|
||||